EDF begins inquiry into stress corrosion “root causes”

(Montel) EDF has launched an in-depth inquiry into reactor stress corrosion cracking, the utility and France’s nuclear safety authority (ASNR) said on Thursday.

Published

“EDF has indeed launched such a programme”, which aims “to better understand the parameters that influence the initiation and propagation of cracks”, an ASNR spokeswoman told Montel, after stress corrosion recently reappeared on reactor Civaux2 (1.5 GW) in a pipe section replaced only two years ago.

The inquiry would notably “further investigate a potential link between dissolved oxygen and corrosion”, an EDF spokeswoman said.

So far, the main reasons identified for stress corrosion were the design of affected pipes and repairs carried out on certain welds during construction, an ASNR spokeswoman told Montel. She added that a “possible influence of oxygen levels in the fluid” was also being explored, though this had yet to be confirmed.

Montel Markets


Get everything included in Free access, plus full Montel News and energy price data in one platform.

Built for professionals who need real-time market intelligence, deeper insight, and a complete view of European energy markets.

14-day free trial

Full news coverage and price data for faster decisions

  • Everything included in Free access
  • Full access to all Montel News content, including breaking news and long reads
  • Live and historical price data across European energy markets
  • Coverage across power, gas, carbon, Guarantees of Origin, LNG, oil and coal
  • Personalised dashboards and market monitoring tools
  • Fast browser and email alerts for key market developments

Start your free trial

Powered by Labrador CMS